Masterbatch condutor para polímeros PP PS PE

Masterbatch condutor para polímeros PP PS PE

Masterbatch condutor para polímeros é um composto formulado com preto de carbono, nanotubos de carbono ou grafeno para atender aos requisitos de proteção de ESD e obter descarga eletrostática .
Enviar inquérito

Descrição dos produtos

 

Conductive Masterbatch For Polymers is a compound formulated with carbon black, carbon nanotubes or graphene to meet ESD protection requirements and achieve electrostatic discharge. The conductive filler of carbon black conductive masterbatch is carbon black, which is one of the most widely used functional fillers for ESD plastics, and it always provides conductivity to conductive masterbatch for ESD protection. Carbon black can also be used as a medium-low-cost pigment to produce various shades of black on the final product, which can be combined with a variety of carrier resins such as ABS, HIPS, PP, PE, POM, PC and PA to produce conductive compounds. Carbon nanotube-based masterbatch and graphene-based conductive masterbatch can be used in high-purity applications and have little effect on shrinkage or mechanical properties compared to carbon black-based conductive Masterbatch . nanotubos de carbono são estruturas ocas compostas por cilindros de grafeno de átomos de carbono tampados nas duas extremidades . baseado em nanotubos de carbono e masterbatches baseados em grafeno fornecem baixa resistividade superficial em níveis de carga muito baixos .}}}}}}

HIPS ABS ABS ALIGADO MASTERBATCH

O MasterBatch condutor é baseado na resina de poliestireno como transportadora, com nanotubos de preto e carbono de carbono, que podem fornecer proteção de descarga eletrostática ideal, com um SR de 10E 2-10 e4 ohms/sheets . este MasterBatch pode ser mixado em seco e extrudido em sheets. 40%-60%, e também pode ser usado como material condutor .

Ldpe hdpe condutive masterbatch

O MasterBatch condutor é baseado na resina PE como transportadora e com preto de carbono, que pode alcançar a interferência eletromagnética condutora (EMI) de interferência eletromagnética (EMI) e outras funções ..}, a força de realização é desenvolvida especialmente para os fadios altos e com fadios altos.}}.}}.}} de uma fadiga de ruptura e a fadrinha alta.}.}.} a força de falha.}.}.}.} força masterbatch é especialmente desenvolvida para os falhas de plástico altamente flexível e com fadões altos e extremamente flexíveis e altos e com fadios altos.}.. MasterBatch fornece proteção ideal de descarga eletrostática, com um SR de 10E 3-10 e5 ohms/quadrado .

PP FOLHA MASTERBATCH

This conductive masterbatch is based on PP resin as a carrier and with carbon black to prevent the polymer from decomposing during molding or extrusion. This masterbatch provides ideal electrostatic discharge protection with an SR of 10E2 – 10E6 ohms/sq. The decay rate of this masterbatch is measured in nanoseconds, which is sufficient to provide a grounding path and release a stronger Charge . Este masterbatch condutor é adequado para processamento e fabricação de extrusão de folhas PP PP .

Masterbatch condutor específico para PC

Using PC resin as a carrier and adding carbon nanotubes, this conductive masterbatch is suitable for plastic products with anti-static, electrostatic dissipative, dust-proof, conductive electromagnetic interference (EMI) shielding and other properties. The SR of the conductive masterbatch is 10E4-10E5 Ohms/sq. It can be added Na proporção e depois pela injeção moldada ., é um masterbatch condutor de alto desempenho e custo-benefício .

Propriedades do Polymer condutive Masterbatch

- A condutividade varia de 10^1 a 10^6 ohms/sq

- dosagem ajustável para melhorar o desempenho antistático .

- Compatível com uma variedade de matrizes .

- Fácil de dispersar, molde de injeção ou extrude .

- Todos os produtos são compatíveis com ROHS .

Vantagens da tecnologia Tanfeng

More cost-effective than competitors: Permanent antistatic agent and permanent antistatic masterbatch are our best-selling products. Our market price is three-quarters of that of competitors, which can save customers 25% of costs. Permanent antistatic agent is an important component of ESD plastic materials. It is a chemical substance that can effectively give materials long-term antistatic properties. It is different from traditional antistatic agents. The effect of traditional antistatic agents may weaken over time or changes in usage conditions, while permanent antistatic agents can maintain a stable antistatic effect throughout the service life of the material. Permanent antistatic masterbatch is a granular substance made by mixing antistatic agent and carrier resin in a certain proportion Através de um processo específico ., sua principal função é facilitar a adição uniforme de agente antistático durante o processamento do material, para que o produto final tenha propriedades antistáticas boas e estáveis ​​.

 

 

 

Tag: Masterbatch condutor para polímeros PP PS PE, China Masterbatch para polímeros PP Fabricantes, fornecedores, fornecedores, fábrica, Masterbatch antiestático, Partículas plásticas condutivas de nanotubos de carbono, Compostos condutores MasterBatches, Masterbatch condutor para polímeros PP PS PE, PA66 Nanotubo de carbono MasterBatch, PPS carbono nanotubo condutor masterbatch