Conductive pastes are the foundation for the development of electronic components and are key materials for packaging, electrodes and interconnections. They are high-tech electronic functional materials integrating metallurgy, chemical engineering and electronic technology, and are mainly used in various fields of the electronics industry such as thick film integrated circuits, sensitive components, capacitors, potentiometers, thick film hybrid integrated circuits, and A tecnologia de montagem na superfície . pastas condutivas pode ser classificada em duas categorias principais: pastas condutivas do tipo de sinterização e adesivos condutores do tipo de cura (tintas condutas) . tipo de sinterização pastas condutivas são usadas principalmente para eletrodos de cerâmica eletrônica
Components (such as ceramic capacitors, thermistors, varistors, etc.) and packaging of electronic devices, with sintering temperatures generally ranging from 500 to 1000℃. Curing type conductive adhesives are mainly used for conductive wires of flexible circuits and electronic packaging, with curing temperatures ranging from room temperature to 200℃.
Composição
The conductive paste that conducts electricity through heating is a widely used and commonly utilized type of paste in the electronics industry. Its composition mainly consists of three parts: inorganic binder, conductive filler, and organic carrier, all of which are mixed in a certain proportion. The inorganic binder is commonly referred to as glass powder, which is generally made by melting and Misturando SiO2 e alguns óxidos metálicos em uma determinada proporção . precisa ser extinto e moído antes de ser fabricado . O enchimento condutor é geralmente composto de metais preciosos como Ru, Pd, Au, AG e metais base como Cu, Ni, Zn e ALIVE, 5 {5.}}}}}}.}.}}.}}}.}} {5}. {5}. Embora os metais da base sejam mais propensos à oxidação, portanto, eles geralmente têm uma camada de filme de óxido em sua superfície . se esses metais forem adicionados à pasta condutora e sinterizados a altas temperaturas, esses metais base serão mais propensos à oxidação, o que afetará inevitavelmente a condutividade elétrica da pasta condutiva {{{7 {7. O produto será muito alto ., o transportador orgânico é geralmente um polímero alto molecular, que afeta a propriedade niveladora da pasta . boa propriedade de nivelamento significa que o vedação após a ligação é denso sem os orifícios do ar, e o desempenho elétrico será relativamente estável; Por outro lado, se a propriedade niveladora da pasta for ruim, haverá vários defeitos, como orifícios e rachaduras após a sinterização, causando um desempenho elétrico ruim do sistema de ligação . atualmente, os portadores orgânicos mais usados são geralmente resina epoxi, álcool de cânfora e etillulose {}}}
Mecanismo condutor
A pasta condutora do tipo de sinterização consiste principalmente de adesivos inorgânicos, enchimentos condutores, portadores orgânicos e outros aditivos funcionais . depois de serem secos a baixa temperatura e sinterizados em alta temperatura, a pasta contém apenas os adesivos inorgânicos e os presos .} the inorganic is sintered at high temperature and cooled down, it shrinks, causing the conductive particles to come into contact with each other, thereby conducting electricity. Similarly, like Chemicalbook, the conductive adhesive conducts electricity because the epoxy resin and other polymers solidify and cause the conductive fillers to come into contact with each other. Whether it is the sintering conductive paste or the cured Adesivo condutor, eles não são condutores antes de serem sinterizados e curados . O principal motivo é que não há contato mútuo entre as partículas condutoras e nenhum canal condutor foi formado . somente após serem sinterizados ou curados, a forma do canal condutor e, portanto, conduz a eletricidade.
Processo de preparação
1. For the preparation process of the sintering infiltration type conductive paste, taking silver paste as an example, the process of preparing the paste is explained. First, according to the formula, silver powder and glass powder are weighed. The silver powder and glass powder are mixed evenly and then added to the organic carrier while stirring. This only obtém inicialmente a pasta de prata condutora porque a distribuição de cada componente na pasta não é suficientemente uniforme ., deve ser uniforme . principalmente, métodos como a moagem de bolas químicas ou a moagem de três rolagem são usadas para a máquina de moagem de três roll em 7.. uniforme .
2. Processo de preparação de cura o adesivo condutor após pesar com precisão o preenchimento condutor, resina epóxi, agente de cura e outros aditivos funcionais em uma certa proporção, misture e mexa para uniformizar o sistema ., teste o desempenho e o pacote para armazenamento .
Principais parâmetros de desempenho
1. condutividade da pasta A condutividade da pasta é um dos principais parâmetros da pasta ., existem muitos fatores que afetam a condutividade da pasta, incluindo os tipos de partículas condutivas e os adesivos correspondentes, a quantidade de pó condutivo, ‘2» e o sintering/cura do processo de partícula, e o sintering/cura do processo de partículas, e o sintering/cura e a quantidade de pó condutiva, e a forma e a forma »2» e os seguintes e os seguintes e os adesivos e os seguintes {a quantidade de partículas »} e os adesivos correspondentes, a quantidade de pó condutivo,‘ 2 e a forma »e a forma» 2 de cocô e a quantidade de pó condutor, e a forma de »e a forma de» e a forma »2» e a quantidade de partículas.
2. molhar a propriedade de pasta condutora A propriedade umedecida da pasta condutora refere -se à afinidade do líquido à superfície sólida . Isso examina se a pasta condutora pode ser efetivamente espalhada quando o químico do pó por pó é mais eficaz no subtrato ‘» quando »quando o pó da química (e também pode ser o pó por pó por pó). A tensão superficial do vidro durante o derretimento . boa propriedade umedecionada é uma condição para a disseminação eficaz, e essa condição também é um dos fatores -chave para concluir com êxito a conexão eficaz . A propriedade de umedecimento é examinada principalmente pelo ângulo de contato .}
3. adesão da pasta condutora A adesão da pasta condutora é a força de tração que a pasta pode suportar por unidade de área . As fontes de adesão incluem principalmente força de ligação química, força intermolecular, atração eletrostática interfacial e força mecânica {2.}}}}}}}}}}}}